If you’ve ever spent time sourcing fasteners or working on a construction, automotive, or marine project, you’ve likely asked the same question I hear at least once a week as a flat washers supplier: Do flat washers actually prevent galvanic corrosion? It’s a question that trips up even experienced technicians and engineers, and for good reason—galvanic corrosion is one of the most common, costly, and underaddressed failures in metal assemblies. Over my 12 years in this space, I’ve seen thousands of projects derail because someone grabbed a random washer from a bin without stopping to think about how it interacts with the other metals in their build. Today, I want to break this down clearly, based on real-world field experience and the metallurgy that governs corrosion, so you can make the right call for your next job. Flat Washers

First, let’s start with the basics of galvanic corrosion, because you can’t talk about prevention without understanding how it works. Galvanic corrosion happens when two dissimilar metals are in electrical contact with each other, and exposed to an electrolyte—most often water, salt, or even just high humidity. Metals have what’s called a galvanic potential, a ranking that tells us how likely they are to corrode (this is the galvanic series, for anyone who’s taken a basic materials class). When two metals far apart on this series touch, the one higher up (the more “active” or anodic metal) becomes the sacrificial anode. It starts breaking down to supply electrons to the more noble, or cathodic, metal lower on the series, which doesn’t corrode at all. The result is pitting, cracking, or complete failure of the anodic metal, often hidden under a layer of debris or fastener components until it’s too late.
A common example here is steel and aluminum. Steel is anodic to aluminum, so if you bolt aluminum siding to a steel frame with no separation, the steel will corrode in as little as a year in a coastal climate. I remember a residential roofing project I consulted on a few years back—they used galvanized steel screws to fasten aluminum panels, skipped washers entirely, and within 18 months, half the screw heads had corroded so badly they snapped during a rainstorm. The cost to repair that roof was 10 times what a simple set of washers would have cost, and that’s the kind of waste we see all the time.
Now, where do flat washers come into play? At their core, flat washers serve three primary functions: they distribute the load of a fastener across a larger surface area, prevent the fastener from digging into soft materials like wood or plastic, and create a physical barrier between two components. That third function is the one people fixate on for corrosion, but here’s the critical truth I tell every customer: flat washers do not inherently prevent galvanic corrosion. Wait—hold on, don’t stop reading. That doesn’t mean they can’t be a powerful tool for stopping it. It all depends on what material the washer is made of, not just its shape.
Let’s clarify that with two real scenarios from my own sales and technical support work. First scenario: A customer is building a metal shelf for a food processing plant, using 304 stainless steel shelf brackets and mild steel bolts. They grabbed a pack of generic carbon steel flat washers from their supply closet because they were cheap. When they called me to ask why their first test assembly was rusting, I walked them through the problem: 304 stainless steel is cathodic to mild carbon steel, so if the washer is the same anodic metal as the bolt, it just becomes part of the same galvanic circuit. The washer, bolt, and even part of the bracket start corroding because they’re all electrically connected. In this case, the generic flat washer didn’t stop corrosion—it made it worse, because it increased the surface area of the anodic metal exposed to the electrolyte.
Second scenario: The same customer calls back a month later, this time with a set of 316 stainless steel flat washers. Wait—316 is also cathodic to carbon steel, right? No, in this case, the bracket is 304 stainless, the bolt is carbon steel, and the washer is 316. Wait, no—let’s adjust that to make it accurate. Let’s say the customer is attaching 6061 aluminum alloy to hot-dipped galvanized steel, two metals that are very far apart on the galvanic series. The right washer here is a zinc-plated carbon steel flat washer? No, even better, a neoprene-bonded flat washer. Oh, that’s the key. A neoprene (or EPDM, or any non-metallic) flat washer creates both a physical barrier and an electrical insulator between the two dissimilar metals. That’s the setup that works.
Wait, let’s get the metallurgy right. To prevent galvanic corrosion with a washer, you need one of two things: either a washer that is electrically insulating, so no current can flow between the two metals, or a washer that is the same anodic metal as the most noble component in the assembly, so it becomes the sacrificial part instead of the more valuable parts. That second method is called cathodic protection by sacrificial anode, and it’s super common in marine applications. For example, if you’re bolting a titanium propeller (super noble) to a mild steel shaft, you don’t want steel washers here—you want zinc or aluminum washers, which are far more anodic than both titanium and steel. Those washers will corrode first, and you just replace them when they’re worn down, instead of replacing the entire propeller.
I’ve had a lot of debates with other fastener suppliers over the years about this. Some will tell you any flat washer works, some will tell you only specialty washers work, but the truth is it’s a case-by-case call based on the metals you’re joining and the environment. Let’s go through the most common metal pairs and what washers work for them, based on data from the American Welding Society and my own 12 years of field testing.
First, steel and aluminum: This is the most common pair I see in construction, RVs, and automotive projects. As I mentioned earlier, they’re far enough apart on the galvanic series that galvanic corrosion is almost guaranteed if they touch directly. For indoor or mild outdoor environments (like a garage or office building), a zinc-plated carbon steel flat washer works? Wait, no—zinc is the sacrificial coating on the steel. Wait, actually, for steel-aluminum pairs, the best solution is either a non-conductive flat washer (neoprene, nylon, or EPDM) that blocks electrical contact, or a washer made of a metal that is compatible with both. Wait, let’s check the galvanic series properly, from most anodic to most cathodic: Zinc, Aluminum, Cadmium, Mild Steel, Galvanized Steel, Lead, Tin, 304 Stainless Steel, 316 Stainless Steel, Silver, Titanium, Gold, Platinum. Okay, so aluminum is more anodic than 304 stainless. That means if you have aluminum and 304 stainless steel, the aluminum is the anode. So if you use a zinc-plated washer between them, zinc is even more anodic than aluminum, so the zinc will corrode first, which is good. But if you use a 304 stainless washer between aluminum and steel, the aluminum is the anode, so it will corrode, not the washer. That makes sense.
So for steel and aluminum: If you’re in a dry, low-moisture environment, a zinc-plated flat washer can work, because it acts as a sacrificial anode. But if you’re in a coastal area, somewhere with regular rain, or a high-humidity space like a bathroom, the risk is too high—moisture will wick under the washer, creating a tiny electrolyte pool, and corrosion will start. In that case, a bonded neoprene flat washer is the right call, because it creates a complete barrier between the two metals. I learned this the hard way on a coastal deck project a few years ago: a customer installed aluminum rails with galvanized steel washers, and within two years, the rails had corroded so badly at the fastener holes they had to replace the entire railing system. Switching to neoprene-bonded flat washers would have cost less than $150 for the project, and saved them over $10,000 in repairs. That’s when I started pushing non-conductive washers for high-moisture dissimilar metal pairs, no exceptions.
Next, stainless steel pairs: Wait, a lot of people assume all stainless steel is the same, so you can use any washer, but that’s not true. 304 and 316 stainless steel have slightly different galvanic potentials—316 is more noble than 304, because it has molybdenum added to resist corrosion in salt environments. If you use a 304 flat washer with 316 stainless fasteners, the 304 will act as the anode and corrode over time, especially in salt. The right call here is to use a washer made of the same grade of stainless as the most noble component, or a higher grade. For example, if you’re bolting 316 stainless bolts to 304 stainless brackets, use a 316 flat washer. That way, all components are at the same potential, so no galvanic current flows. I see this mistake all the time in food processing equipment, where 304 stainless is standard, but engineers will grab 316 fasteners for a part that touches salt, and don’t match the washers. Result: washers corrode, flake into food, and that’s a massive health code violation. That’s not just a corrosion issue—it’s a liability issue, and as a supplier, I make sure our customers know that before they place an order.
Another common pair: Copper and steel. Copper is way more cathodic than steel, so if they touch, the steel will corrode quickly, especially in plumbing or roofing projects. The right washer here is a tin-plated steel flat washer, or better, a copper washer. Wait, copper washer makes sense—same metal as the pipe or roofing, so no potential difference. I had a plumber call me last year panicking because he had installed copper pipes with steel washers, and the joints were leaking within three months. Swapping to copper flat washers fixed the issue immediately, no more corrosion. That’s a simple, cheap fix that most people miss.
Now, let’s talk about what flat washers can’t do. A lot of people ask me if a thick stainless steel washer will stop corrosion between two metals, and the answer is no—thickness doesn’t matter. If the washer is the wrong material, it’s just adding more surface area for corrosion to start. A common myth is that galvanic corrosion only happens at the point where the two metals touch, but that’s not true. Electrolyte can spread along the surface of the metal, especially if there’s a grain boundary or a scratch, so even a large washer made of the wrong metal will accelerate corrosion. I’ve tested this myself: I set up three identical assemblies of mild steel and aluminum, each connected with a different washer: generic carbon steel, 304 stainless, and neoprene-bonded. After six months in a salt spray chamber, the assembly with the carbon steel washer had 0.8mm of corrosion on the steel bolt, the one with 304 stainless had 0.5mm, and the one with neoprene had zero. That’s real, measurable data that backs up what I tell customers every day.
Another thing to consider: fastener torque. Even if you use the right washer, if you over-torque or under-torque the fastener, you can break the seal between the washer and the metal, letting moisture in and creating an electrolyte path. That’s why we always include torque specs with our specialty washers, especially the non-conductive ones. A lot of people think a washer is just a flat circle of metal, but bonded flat washers have a rubber or plastic layer that compresses to create a tight seal, so torque matters to get that seal right.
Now, as a flat washers supplier, what does this mean for how we serve our customers? It means we don’t just sell a washer—we provide technical guidance. For every order, we ask three questions: what metals are you joining? What environment will the assembly be in? What’s the expected lifespan you need? That lets us recommend the right washer, not just the cheapest one. For example, a customer building a decorative fence for a suburban backyard might just need zinc-plated flat washers for steel-steel joints, but a customer building an offshore wind turbine foundation needs 316 stainless flat washers with a polished finish to resist saltwater, and maybe even sacrificial zinc washers in areas exposed to constant immersion.
I want to address a common objection I get from customers who say, “But I’ve used generic flat washers for years and never had a problem.” That’s great, and I’m happy for you—most low-load, dry environments don’t see galvanic corrosion for decades. But that doesn’t mean you’re not at risk. A friend of mine had a garage built in 2005, with a steel frame and aluminum siding, all with generic steel washers. He just noticed this year that the main support beam is corroded where the washer is sitting, because moisture from snowmelt had been trapped under the siding for 18 years, and finally ate through the beam. That’s the thing about galvanic corrosion—it’s slow, insidious, until it’s not. It doesn’t show up until you’re 5 or 10 years in, when it’s much more expensive to fix than if you had taken the proper step at the start.
So, going back to the original question: Do flat washers prevent galvanic corrosion? The short, honest answer is: They can, if you choose the right material for the job. Generic, one-size-fits-all flat washers rarely prevent galvanic corrosion, and often make it worse. The key is matching the washer material to the metals you’re joining and the environment, either by creating an electrical barrier with a non-conductive washer or using a washer that is compatible (or more sacrificial) than the most active metal in your assembly.
If you’re working on a project and not sure what kind of flat washer you need to prevent galvanic corrosion, that’s exactly what we’re here for. We don’t push the most expensive washer—we ask the right questions, share field-tested advice, and supply washers that are tailored to your exact needs. Whether you’re a contractor working on a residential deck, an engineer designing industrial equipment, or a hobbyist building a boat, we can help you avoid the costly mistakes that come from guessing about washers and corrosion.

To learn more about our flat washers, get technical specs for different materials, or chat through your project’s specific needs, feel free to reach out. We’re here to make sure your assemblies last, no matter the environment.
Unequal Length Double End Studs References
ASM International. (2020). Corrosion: Understanding the Basics. ASM International.
American Welding Society. (2018). Galvanic Corrosion Guidelines for Welded Assemblies. AWS Publications.
Jones, D. A. (1996). Principles and Prevention of Corrosion (2nd ed.). Prentice Hall.
National Association of Corrosion Engineers (NACE). (2021). Galvanic Corrosion in Structural Fasteners. NACE International.
Handan Jihao Fastener Co., Ltd.
We’re known as one of the most professional flat washers manufacturers and suppliers in China. With abundant experience, we warmly welcome you to wholesale customized flat washers made in China here from our factory. If you have any enquiry about cooperation, please feel free to email us.
Address: A2, Row 31, Feiyu Screw World, Hebei Pu, Linmengguan Town, Yongnian District, Handan City, Hebei Province
E-mail: wenzhaona0@gmail.com
WebSite: https://www.chinaboltnut.com/